C15000 Zirconium Copper Bar

본문 바로가기


Home > Product > C15000 Zirconium Copper Bar
Selling leads
C15000 Zirconium Copper Bar
Posting date : Jan 05, 2017
Membership
Free Member Scince Jan 03, 2017
FOB Price
8.9USD/KG
Min. Order Quantity
100KG
Supply Abillity
50MT/MONTH
Port
SHANGHAI
Payment Terms
T/T
Package
WOODEN CASE
Keyword :
Category
Contact
Steven
Selling Leads Detail
Company Info
 
Quick Detail
Place of Origin
China [CN]
Brand Name
CANHU/OEM
HS-CODE
-
Package & Delivery Lead Time
Package
WOODEN CASE
Delivery Lead Time
15 DAYS
Detailed Description
CuZr – UNS.C15000 Zirconium Copper is an excellent and unique copper alloy with high electrical conductivity, hardness, and ductility, moderate strength, and excellent resistance to softening at elevated temperatures.  The addition of 0.15% zirconium (Zr) to copper results in a heat treatable copper alloy which may be solution treated and subsequently aged to produce these desirable properties.  Rod is supplied from the mill in the fully aged and drawn condition so no further heat treatment is required by the fabricator.  The softening temperature of properly heat treated C15000 rod exceeds 500°C as compared to unalloyed, pure copper which softens at 200°C and silver bearing coppers which soften at 350°C.
Typical Application for C15000 Zirconium Copper Alloys:
Electrical Industry: Resistance Welding Electrodes, Circuit Breaker Switches, Stud Bases for Power Transmitters, Rectifiers, Diodes, Switches, CommutatorsConsumer: Rod Extensions, Pencil-type, Light Soldering Guns, TipsIndustrial: Connectors, Solderless Wrapped, Welding Wheels, Resistance Welding Tips
Available Sizes:Custom Diameter & Sizes, Random Mill lengths
Available Products (forms):Round bars, Flat bars, Square bars, Rectangular bars, Hexagon bars, PlatesCustom shapes are available upon request.
Chemical Composition:
Zr: 0.15-0.20%Cu: BalanceNote: Copper plus additions equal 99.90% minimum.
Typical Physical Properties:Density at 68°F: 0.321 Lbs./In.3Specific Gravity: 8.89Melting Point (Liquidus): 1080°C (1976°F)               (Solidus): 980°C (1796°F)Coefficient of Thermal Expansion per °F: 9.4 x 10-6 (68-212°F)9.8 x 10-6 (68-572°F)11.2 x 10-6 (68-1200°F)Electrical Conductivity at 68°F (volumetric): 85-95% IACS (aged and drawn)                                               55-72% IACS (solution annealed)Thermal Conductivity Btu/ft.2/ft./hr./°F at 68°F: 212Modulus of Elasticity - Tension: 18,700 ksi
Note: 1). the units are based upon US Customary.2). the typical physical properties apply to age hardened products.
International Specification:
Rods/Bars/Plates/Sheets: UNS.C15000, RWMA Class 1, SAE J461,463; ISO5182-1991
European Standards: CuZr, DIN 2.1580, CW120C to EN
Note: ASTM: American Society for Testing and Materials SAE: Society of Automotive Engineers RWMA: Resistance Welder Manufacturers' Association Note: Unless otherwise specified, material will be produced to ISO & RWMA.
Mechanical Properties:The detailed Mechanical Properties will be available on request from customers.

ECROBOT CO., Ltd, Business Registration Number : 220-88-71747, CEO J.W.Park, TEL : +82-2-552-7676, E-mail : E-mail : Contact us
Address : (Hwanghwa B/D 11F, Yeoksam-dong)320, Gangnam-daero, Gangnam-gu, Seoul, South Korea
About Us Privacy Policy Terms of use Copyright © 2000-2024 ECROBOT.COM. All rights reserved.
Top